Application · Appliances
Antibacterial plastics for appliances: efficacy, yellowing and durability
The short answer: white-good liners and housings use a zinc-oxide masterbatch system — ZnO 40%, dosed at 2–4% in the compound, ≥90% efficacy, ΔE ≤ 1.5 after 200 °C × 30 min — the most reliable option on the "antibacterial without yellowing" axis. For ≥99% or dark parts, move to silver or a silver–zinc hybrid; liners, baby products and food-contact parts must clear the GB 4806 route first. Quoting efficacy alone, without colour and durability data, is the classic appliance-project failure.
Himing New Material (Zhongshan CSII) Co., Ltd. · IATF 16949 · ISO 9001 · CRCC · Zhongshan, Guangdong
1. Six requirements on an antibacterial part
Efficacy is the entry ticket; colour and durability decide whether it ships.
| Requirement | Typical criterion | What it drives |
|---|---|---|
| Efficacy | GB/T 31402 / ISO 22196 | ≥90% and ≥99% are different tiers — confirm what the appliance standard requires before quoting |
| Colour after processing | ΔE ≤ 1.5 at 200 °C × 30 min | The most common failure on white goods: an additive that cannot take the temperature yellows the whole batch |
| Durability | Re-test after wiping / ageing | Ask for retained activity after 500 wipes or ageing, not only the ex-works number |
| Safety & compliance | GB 4806 (food contact) / silver migration | Liners, baby products and tableware need the food-contact compliance route |
| Standard basis | GB/T 21551.2-2024 | The appliance antibacterial standard changes test organisms and evaluation; validate decay against the new edition |
| Appearance & odour | Colour shift, odour, plate-out | Zinc systems are milder; high silver loadings raise both colour and migration risk |
2. Five options compared
Efficacy per GB/T 31402 / ISO 22196; colour values are typical after 200 °C × 30 min.
| Option | Efficacy | Colour after processing | Main drawback | Fit |
|---|---|---|---|---|
| Zinc oxide masterbatch | ≥90% (tunable) | ΔE ≤ 1.5 | Good heat stability, lower cost, white-part friendly | Fridge liners, washer parts, sanitary ware, baby products |
| Silver-based | ≥99% | Colour shift at high load | High efficacy; cost and discolouration rise together | High-efficacy demands, dark parts |
| Silver–zinc hybrid | ≥99% | Manageable | Balances efficacy and appearance; most complex formulation | White parts needing 99% |
| Post-coating antibacterial | Coating-dependent | Coating-dependent | Poor abrasion and durability; failure follows coating loss | Not for long-term contact parts |
| In-house masterbatch blending | Depends on ratio | High risk | Poor dispersion causes local failure and colour variation | Only with proven dosing experience |
3. Why white goods start with zinc
- Heat: colour shift stays controlled in a 200 °C window, so white batches do not yellow.
- Compliance: a simpler migration path for food-contact and baby products.
- Cost: less additive is needed to reach ≥90% than with silver.
- Dispersion: delivered as a 40% ZnO masterbatch dosed at 2–4%, more uniform than dry powder blending.
- Boundary: at ≥99% zinc alone is not enough — use a silver–zinc hybrid and re-validate colour.
4. Matching Himing products
Two routes: buy the masterbatch to dose into your own compound, or buy the finished compound.
ZnO 40% system dosed at 2–4%, ≥90% efficacy, ΔE ≤ 1.5 — appliances, sanitary ware, baby products.
View details →For dosing into an existing formulation; 25 kg minimum, carrier and spectrum customisable.
View details →5. Questions buyers ask
Is 90% efficacy enough?+
Why do white parts go yellow?+
Is silver safe?+
How do you verify a five-year claim?+
Send the part, the efficacy target and the colour