Insight · Material selection

Choosing glass content: GF15, GF30, GF35 or GF50

8 November 2026 · Himing New Material (Zhongshan CSII) Co., Ltd.

The short answer: glass content should follow four inputs — allowed deflection, impact floor, wall thickness and cosmetic grade — not "more is stronger". Most structural parts are satisfied at GF30; GF35 suits load and fatigue duty; GF50 belongs to high-stiffness, low-impact, dimension-critical work. Each step up buys stiffness and heat resistance and pays with toughness, flow and surface.

1. Four levels, measured and typical

ContentTensileFlex modulusImpactFlowSurfaceTypical use
GF15~100–120 MPa~5,000–6,000 MPaHighGoodSlightCosmetic parts, thin walls, tough structures
GF30123 MPa (PA6 FR) / 155 MPa (PA66)7,200–8,600 MPaMediumMediumVisibleGeneral structures, brackets, housings
GF35191 MPa (PA66)8,713 MPaLower but higher absolutePoorPronouncedHeavy-duty structures, rail fastenings
GF50~220–240 MPa~14,000–16,000 MPaLowVery poorSevereHigh stiffness, low impact, dimension-critical

Figures in context are our measured typicals (GF30 PA66 155 MPa / 7,200 MPa, GF35 PA66 191 MPa / 8,713 MPa, FR PA6 GF30 123 MPa / 8,600 MPa); other values are industry-typical ranges and indicative only. The grade TDS governs.

2. A four-step method

01
Start from the stiffness requirement

Work back from the allowed deflection to the modulus you need, then see which GF level clears it. Many parts are fine at GF30; moving to GF50 only adds cost and fibre read-through.

02
Then set the impact floor

Notched impact falls as glass rises. Parts with clips, threads or assembly impact need margin — use an impact-modified system rather than dropping glass content blindly.

03
Check flow against wall thickness

Above GF35 flow drops sharply; long, thin parts risk short shots and weak weld lines. Run a flow analysis before fixing the content.

04
Decide the cosmetic requirement last

Paint-free surfaces are sensitive to fibre read-through. If appearance leads, drop to GF15–20 or use a low-read-through package; process alone will not hide GF30.

3. Three common misjudgements

  1. Selecting on tensile strength alone. High tensile does not stop parts breaking — clips, threads and assembly cracks are impact and weld-line failures.
  2. Ignoring weld lines. Fibres orient unfavourably at a weld line, so local strength can be 30–50% of the bulk. Design load-bearing welds on that basis.
  3. Blaming the material for warpage. Anisotropy comes from orientation; without gate and mould-temperature changes you are only trading one warpage figure for another.

4. Matching grades

5. Questions engineers ask

Does more glass always mean higher strength?+
Tensile and modulus usually rise with content, but impact toughness, elongation and flow fall. Near GF50 the material is brittle and weld-line strength is low, so real parts can fail earlier in assembly or impact. Choose the lowest level that meets the requirement.
Why does adding glass make parts warp more?+
Fibres orient with the flow, so shrinkage differs between flow and cross-flow directions. The higher the content, the thinner and longer the part, the stronger the anisotropy. Fix it with gate position, mould temperature, packing and design — a grade change rarely helps.
How much difference does GF30 versus GF35 make?+
In our measured PA66 systems, tensile moves from 155 to 191 MPa and modulus from 7,200 to 8,713 MPa — about 20%, enough to change the safety factor on a load-bearing part. Flow and read-through get worse at the same time, so it depends on the stress level in the part.
Can processing eliminate fibre read-through?+
It can be reduced, not eliminated. Higher mould temperature, revised gating and venting, and adjusted injection speed all help, but GF30 remains visible on cosmetic faces. Only lower glass content or a low-read-through system removes it.

Next: send the part, the allowed deflection and the impact requirement, and we will work back to a glass content from those four inputs instead of quoting a grade name.