Application · Automotive

Under-hood compounds: fix the local temperature first

The short answer: conventional structural parts run on PA66 + 30% GF — tensile 155 MPa, flexural 235 MPa, modulus 7,200 MPa, notched impact 14 kJ/m². Where load and fatigue demand more, move to PA66 + 35% GF (191 MPa / 8,713 MPa); above 180 °C or near the exhaust, use PA46. What decides success is rarely the grade name — it is retention after heat ageing, behaviour after oil immersion, and warpage from fibre orientation.

Himing New Material (Zhongshan CSII) Co., Ltd. · IATF 16949 · ISO 9001 · CRCC · Zhongshan, Guangdong

1. Six constraints inside the bay

One engine bay, several material classes — by location.

RequirementTypical criterionWhat it drives
Continuous temperatureMeasured rise plus marginLocations in one engine bay differ by 40 °C or more — specify per location, not per vehicle
Retention after ageingRe-test after 1000 h155 MPa as-moulded does not mean 155 MPa after ageing; ask for retention
Oil / coolant resistanceMechanical + dimensional after immersionPA absorbs oil and plasticises; strength and modulus fall together
Vibration fatigueBench test to the vehicle spectrumFibre orientation and weld lines decide fatigue life more than the grade does
Dimensional stability / warpageOrientation and mould temperatureAbove GF30 anisotropy is significant; long thin parts need a warpage plan
Flame / CTIOnly where the circuit requiresNot every under-hood part needs V-0 — it follows the electrical standard, not the bay

2. Five options compared

Tensile values are dry, as-moulded; hot, wet and aged values must be tested for the duty cycle.

OptionTensileHDTMain drawbackFit
PA66 + 30% GF, structural155 MPa~250 °CBest cost/performance; retention drops above 150 °C long-termCovers, brackets, water chambers, sensor housings
PA66 + 35% GF, heavy duty191 MPa~255 °CBetter stiffness and fatigue; lower flow, more warpage sensitivityLoad-bearing brackets, structural reinforcement
PA46—~280 °CHighest heat; high moisture uptake, highest costNear exhaust/turbo, connectors
PPA (custom)—~260 °CLow moisture uptake, good fluid resistance; costly, long lead timeHot-humid, dimension-critical parts
Die-cast aluminium——No temperature ceiling; heavy, high tooling and machining costExtreme heat or very high stiffness

3. Three misjudgements

  1. Using as-moulded strength as the design value. Select on retention after 1000 h; the initial number only ranks candidates.
  2. Ignoring fluids. Oil, coolant and cleaners all shift PA mechanics and dimensions — parts exposed to them need their own safety factor.
  3. Treating warpage as a material problem. Anisotropy above GF30 is structural; without gate and mould-temperature changes, swapping grades will not hold the part flat.

5. Questions engineers ask

At 150 °C continuous, PA66+GF30 or PA46?+
Start from the location and the ageing requirement. PA66+GF30 near 150 °C long-term has to be justified by retention after 1000 h; if retention is short, go to GF35 or PA46. PA46 takes more heat but absorbs more moisture, so dimension-critical parts need that assessed too.
How much strength is lost after oil immersion?+
It depends on base resin, glass content and temperature — there is no universal number. We run immersion to the customer fluid and temperature and report tensile and modulus before and after. If you only have a grade name and no fluid conditions, ask for the severest case first.
Same material, why does their part not warp?+
Fibre orientation drives anisotropy. Gate position, flow length, mould temperature and packing all change orientation, most visibly on long thin parts. That is a structure and process problem; changing grade usually will not fix it — run a flow analysis together.
Do under-hood parts have to be flame retardant?+
Not necessarily. The requirement comes from the electrical safety standard governing the circuit, not from the bay environment. Only parts near electrical connections or covered by an explicit vehicle requirement need V-0; the rest are selected on heat, fluids and fatigue.

Send the location temperature and the fluids

A base-resin and glass-content recommendation within 24 hours; samples from 500 kg in 7–10 days.